We have developed a microcantilever torque magnetometer based on a torsion-mode atomic force microscope. Thin magnetic films are deposited directly onto micromachined silicon cantilevers. We have measured hysteresis loops of iron thin films with thicknesses ranging from 1 to 40 nm and total magnetic volumes ranging from 2.2×10−11 to 8.8×10−10 cm3. The magnetic moment sensitivity is estimated to be 1.3×10−12 A m2/Hz1/2 at room temperature and ambient conditions. We expect that by operating at the cantilever torsion resonance frequency and at higher torque fields sensitivity will be improved by a factor of 100–1000.