Answers are grounded in this paper and cite their sources.
Two kerolite and one garnierite samples were subjected to progressive heat treatments prior to their examination by infrared spectroscopy (IR) in the 1200-600-cm−1 and 3800-3000-cm−1 regions. The heat treatment of the garnierite (a mixture of nepouite and pimelite) selectively dehydroxylated the nepouite thus allowing an examination to be made of the OH-vibration bands due to the pimelite. Both the relative intensities of the 710-670-cm−1 doublet and of the different OH-stretching bands indicated the Ni content of this pimelite to be about 70%. The heat treatments did not modify the 1200-600-cm−1 region of the spectra of kerolites but caused a noticeable sharpening in the OH-stretching region. The relative intensities of the structural OH-stretching bands of dehydrated kerolites showed that they differ from Ni-talcs of similar composition in the distribution of Ni and Mg in the octahedral sites. These cations are randomly distributed in Ni-talc but are mainly segregated into Mg and Ni domains in kerolite. Changes in sharpness, intensity, and position of the structural OH-stretching bands of the kerolites as temperature increases and dehydration progresses are similar to those undergone by Mg- or Li-saturated trioctahedral smectites. Also thermal analysis curves of these minerals show similarities with those of Mg- and Ni-saturated smectites, and suggest that in kerolites too, the hydration water is associated with interlayer (though non-exchangeable) Ni and/or Mg cations.
No takes yet. Share an insight, caveat, or question.
Gérard et al. (1983) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: