The effect of finish rolling temperature was investigated on texture formation in a plain C and a 0.034% Nb microalloyed steel. When finish rolled at 1020°C (i.e. within the γ recrystallization range), the textures in both steels contain the {001}<110> and {110}<110> components. The sharpness of the {001}<110> component generally increases with decreasing finish rolling temperature down to 630°C, while the {110}<110> component gradually weakens and finally disappears after ferrite rolling. The microalloyed steel displays much sharper texture than the plain C steel when finish rolled at 870°C (i.e. within the γ pancaking range for the Nb steel) and at 730°C (in the γ+α intercritical range). After finish rolling at 870°C, the major texture components in the microalloyed steel are {113}<110> and {332}<113>, in addition to the above two, while the plain C steel texture only contains some low intensity maxima. When finish rolled at 730°C, weak peaks appear at {223}<110> and {554}<225> in the plain C steel and stronger ones at {4411}<110> and {554}<225> in the microalloyed steel. After warm rolling at 630°C, the major texture components in both steels are {223}<110>, {554}<225> and {001}<110>.The {001}<110> and {110}<110> components are obtained, by transformation, from the {100}<001> (cube) and {122}<212> (twinned cube) components of the recrystallized γ. By contrast, the {113}<110> and {332}<113> components originate, respectively, from the {112}<111> (copper) and {110}<112> (brass) components of the unrecrystallized γ. During continued rolling in the γ+α or α range, these transformation texture components are further modified by deformation and ultimately give rise to the stable end orientations which constitute the well-known warm rolling texture in steels.
No takes yet. Share an insight, caveat, or question.
Ray et al. (1992) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: