Answers are grounded in this paper and cite their sources.
Si/Pd-based contact schemes based on the solid-phase regrowth (SPR) process have been developed to form low-resistance ohmic contacts to n-Al0.5In0.5P (Eg=2.3 eV) with a minimum contact resistivity of about 6×10−6 Ω cm2. The SPR process responsible for the ohmic contact formation was verified using cross-sectional transmission electron microscopy. The contact resistivity of the Si/Pd-based contacts remained in the range of 2–3×10−5 Ω cm2 after aging at 400 °C for 25 h. Furthermore, a lateral modulation disordering phenomenon as a result of the SPR process in the regrown AlInP layer has been observed. These ohmic contacts may be useful in some novel Al0.5In0.5P-related device fabrication schemes.
No takes yet. Share an insight, caveat, or question.
Hao et al. (1996) studied this question.