Answers are grounded in this paper and cite their sources.
In this study, high performance concrete beams and prisms with high content of PFA were heated to various temperatures up to 450∘C at heating rates of 1∘C/min , 3∘C/min and 10∘C/min . The thermal gradient was found to increase first with the heating time until a peak value was reached and then decrease until the thermal equilibrium was reached, measured as 115∘C , 240∘C and 268∘C for the three heating rates. Spalling occurred on some specimens when the heating temperature was over 400∘C for heating rates of 3∘C/min and 10∘C/min . The hygric gradient was found to reach its maximum when the thermal gradient reached its peak. This study indicates that spalling of HPC could happen when the heating temperature was high enough, and both thermal and hygric gradients reached their maxima.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2016) studied this question.