An attempt for fabricating Fe–Tb–O films with heterogranular structures was made using a soft-solution process with an alternative current for deposition. The resultant film composition was found to be sensitive to the concentration of complex agent, KNaC4H4O6, the intensity i, and the frequency f of deposition current. These dependencies are well explained from the model for film formation. When KNaC4H4O6=283.47 mM, i=6.7 mA/cm2, and f=6 mHz, the film with very high Tb content exceeding 29 at. % were obtained, which exhibited a relatively soft magnetic magnetization of Hc=29 Oe and Mr/Ms=0.93.