Answers are grounded in this paper and cite their sources.
Thin (0.5–5‐ μm) palladium (Pd) membranes were prepared inside pores or on the suface of mesoporous (pore size 4–6 nm), sol – gel‐derived γ‐Al2O3 supports by the chemical vapor deposition (CVD) method using palladium acetylacetonate and palladium chloride (together with hydrogen) as Pd precursors. When Pd is deposited in the form of metal plugs inside pores of γ‐Al2O3, He permeance of the composite membranes increases exponentially with temperature, indicating activated diffusion through the rnicroporous metal deposit defects, while only modest permselectivity for H2 is observed. When Pd is deposited in the form of a metal film on the surface of γ‐Al2O3, He permeance is governed by Knudsen‐viscous flow through meso/macroporous metal film defects. The H2 permeance of different palladium membranes prepared by CVD appears to increase with palladium crystal grain size. The highest H2 permeance and H2:He permselectivity for membranes prepared in this study are about 1.0–2.0 × 10−7 mol·m−2·s−1·Pa−1 and 200–300 at 300°C, respectively.
No takes yet. Share an insight, caveat, or question.
Xomeritakis et al. (1998) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: