The Cs 2 HPO 4 · 2H 2 O single crystals synthesized from an aqueous solution containing equimolar amounts of H 3 PO 4 and Cs 2 CO 3 were studied by impedance and IR spectroscopy, X-ray diffraction analysis, and differential scanning calorimetry (DSC). The IR spectra were analyzed in accordance with the structural data, and the absorption bands were assigned. The proton conductivity was studied at temperatures in the range 20–250°C. The conductivity of dehydrated Cs 2 HPO 4 was low, ~10 –5 –10 –9 S cm –1 at 90–250°C with an activation energy of conductivity E a = 1.1 eV at 130–250°C. The processes determining the character of the temperature dependence of conductivity were consistent with the DSC and thermogravimetry data. According to these data, dehydration of the crystalline hydrate Cs 2 HPO 4 · 2H 2 O starts at 60°C and occurs in three stages, forming Cs 2 HPO 4 · 1.5H 2 O below 100°C; anhydrous Cs 2 HPO 4 at t > 160°C, which is stable up to 300°C; and Cs 4 P 2 O 7 above 330°C.
No takes yet. Share an insight, caveat, or question.
Пономарева et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: