Answers are grounded in this paper and cite their sources.
An ordered mesoporous Mg-Ta mixed oxide (123 m2·g-1 BET surface area, ca. 5.0 nm mesopore size and 3.6 nm wall thickness), which was stable after calcination at 500 °C for 30 h, showed stable and high photo-catalytic activity for overall water decomposition.
No takes yet. Share an insight, caveat, or question.
Uchida et al. (2002) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: