Al 2 O 3f /Al 2 O 3 composites find applications in the aerospace industry due to their high‐temperature resistance, damage tolerance and lower density that encompasses conventional metal alloys. However, current processing that involves slurry impregnation, precursor impregnation and pyrolysis (PIP), etc., tend to damage the fibers due to excessively high sintering temperatures and repeated densification cycles, respectively. Both fabrication methods can introduce defects into the fibers, leading to thermal damage and a reduction in their strength. Thus, this work attempts to modify the PIP process by adding alumina powder during the first impregnation step, followed by subsequent analysis and testing. We find that the alumina precursor utilized in this study underwent a transformation into the stable α‐Al 2 O 3 phase at 1000°C, accompanied by the formation of small and uniformly distributed grain sizes at this temperature. The composite exhibiting the highest flexural strength (112.50 ± 10.23 MPa) was obtained when the first pyrolysis temperature was set at 1000°C and the number of PIP cycles was three, with the fracture mode being characterized as typical non‐brittle fracture. Additionally, the thermal aging performance of the obtained composites was studied. The results indicated that both the strength and toughness of the composites gradually decreased with the extension of thermal aging time. After thermal aging for 108 h at 1000°C in air, the flexural strength of the material decreased from the original 112.50 ± 10.23 MPa to 81.67 ± 7.64 MPa.
No takes yet. Share an insight, caveat, or question.
Yang et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: