This is the authors' abstract. We don't add key points for this paper.
We study the process of interstitial doping of hydrogenated amorphous silicon (a-Si:H) by Li in-diffusion and thermal annealing after Li+ implantation using secondary ion mass spectrometry, dc dark conductivity [σ(T)], electron-spin resonance, and photothermal deflection spectroscopy measurements. All Li-doped a-Si:H samples were characterized by an inhomogeneous distribution of Li atoms. Doping by Li in-diffusion at 230 °C resulted in a Li-rich (up to 1021 cm−3) region at both sample interfaces, a large increase in σ(300 K), and the creation of deep paramagnetic (g=2.0061±0.0002, ΔHp.p.=5.4±0.4 G) defects with defect densities (up to 2×1018 cm−3) proportional to the interfacial Li concentration. Li+ implantation of a-Si:H at 373 K resulted in the creation of deep paramagnetic (g=2.0056±0.001, ΔHp.p.=6.0±0.5 G) defects with defect densities (up to 2×1018 cm−3) proportional to the implanted Li+ dose. Isochronal vacuum annealing of Li+-implanted a-Si:H up to 545 K resulted in an exponential increase of σ(300 K) and an activated (Ea=+0.32 eV) decrease of the spin density with increasing anneal temperatures. Both Li in-diffused and annealed Li+-implanted a-Si:H films displayed thermal equilibration behavior similar to that characteristic of P-doped a-Si:H, which suggests that the defect compensation model of substitutional doping of a-Si:H is also applicable to the case of interstitial doping. However, the defect structure of a-Si:H doped by Li in-diffusion is significantly different than that of both undoped and P-doped a-Si:H due to the precipitation of Li at the interfaces of heavily Li-doped a-Si:H. We discuss the origin of this behavior.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Winer et al. (1989) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: