This is the authors' abstract. We don't add key points for this paper.
The photoluminescence (PL) wavelength of high-purity 0.5-μm-thick metalorganic vapor-phase epitaxy In1−xGaxAs/InP was measured at room temperature (RT) as a function of composition. The relaxed mismatch of these coherently strained layers was between −0.25% and +0.13%, corresponding to x=0.503 – 0.448. The composition was determined by x-ray diffraction (XRD) using a four-crystal monochromator. Extremely narrow XRD linewidths as a function of layer thickness are reported. The PL peak wavelength λp at RT of exactly lattice-matched InGaAs is 1668 nm, corresponding to a band gap Eg=731 meV. The bowing parameter of the strain-free Eg(x) relation is c=−0.494. The measured λp vs x relation agrees well with the strain-free Eg(x) corrected by the hydrostatic part of the strain energy. From line-shape analysis of RT and 77 K PL spectra it is found that the spectra of strained layers contain two lines in accordance with the valence band splitting under uniaxial strain. The conditions for a reliable determination of the compositional homogeneity of large InGaAs wafers by a mapping of λp are given; e.g., a variation Δx=8.7×10−3 over a 2 in. wafer is found.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Kuphal et al. (1993) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: