Niobium carbide thin films were synthesized by atomic layer deposition (ALD) using trimethylaluminum (TMA), NbF 5, and NbCl 5 precursors. In situ quartz crystal microbalance (QCM) measurements performed at 200 and 290 °C revealed controlled, linear deposition with a high growth rate of 5.7 and 4.5 Å/cycle, respectively. The chemical composition, growth rate, structure, and electronic properties of the films were studied over the deposition temperature range 125–350 °C. Varying amounts of impurities, including amorphous carbon (a-C), AlF 3, NbF x, and NbCl x, were found in all samples. A strong growth temperature dependence of film composition, growth rate, and room temperature DC resistivity was observed. Increasing film density, decreasing total impurity concentration, and decreasing resistivity were observed as a function of increasing deposition temperature for films grown with either NbF 5 or NbCl 5 . Superconducting quantum interference device (SQUID) magnetometry measurements down to 1.2 K revealed a superconducting transition at T c = 1.8 K in a 75 nm thick film grown at 350 °C with TMA and NbF 5 . The superconducting critical temperature could be increased up to 3.8 K with additional use of NH 3 during ALD film growth.
No takes yet. Share an insight, caveat, or question.
Klug et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: