Answers are grounded in this paper and cite their sources.
PbTiO3 ceramics with high density and high resistivity have been prepared by adding less than 5 mol % of Bi2/3TiO3, PbZn1/3Nb2/3O3 or their derivatives. These ceramics have dielectric constants of about 200, and can be poled at 200°C under a d. c. field of 40 to 70 kV/cm. The piezoelectric coupling factors k 15, k 33 and k 31 amount to 0.43, 0.35 and 0.068, respectively. The value of k 33 is nearly constant up to the Curie temperature of about 500°C. The aging rate of frequency constant does not exceed 0.1%/time decade. The present ceramics can be used as stable piezoelectric elements in high temperature and high frequency.
No takes yet. Share an insight, caveat, or question.
Ueda et al. (1968) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: