Answers are grounded in this paper and cite their sources.
A new method to obtain high J c Bi-2212/Ag tapes with high reproducibility was developed. Melt-solidifying with Bi2Al4O9 is found to be an effective method for suppressing the vaporization of bismuth oxide during the high-temperature heat treatment. By application of this method, the homogeneity of the microstructure of the Bi-2212 layer was improved considerably due to a decrease of the Bi-poor phase, (Sr, Ca)-Cu-O. The reproducibility of J c values was also improved corresponding to the microstructure, and J c maintained more than 1×105 A/cm2 at 4.2 K in 7 T even for a 1 m tape.
No takes yet. Share an insight, caveat, or question.
Shimoyama et al. (1992) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: