Answers are grounded in this paper and cite their sources.
We evaluated the crystallinities of Ce X Zr1- X O2 (X=0.10–0.20) thin films used as intermediate layer for metal/ferroelectric/insulator/semiconductor field effect transistors (MFIS-FETs), using reflection high-energy electron diffraction (RHEED), X-ray diffraction (XRD) and X-ray pole figure measurement. The crystal alignments of Ce X Zr1- X O2 films on Si(100) were Ce X Zr1- X O2[100]//Si[100] or Ce X Zr1- X O2[100]//Si[001], in the plane. The breakdown field of Ce X Zr1- X O2 was about 3 MV/cm (at I=1 nA/cm2). From C-V measurements, it was found that the electrical properties of the intermediate layers of the MFIS-FETs were good. Oriented perovskite PbTiO3 films were deposited on Ce X Zr1- X O2/Si(100) substrates by digital chemical vapor deposition (CVD). These PbTiO3 films included many PbTiO3 grains aligned with the [100] or [001] axis parallel to the [101] axis of the Ce X Zr1- X O2 crystals at the plane in the PbTiO3/Ce X Zr1- X O2 interface. From C-V measurements of an Al/PbTiO3/Ce X Zr1- X O2/Si(100) sample, we obtained a threshold hysteresis (memory window) of about 1.4 V.
No takes yet. Share an insight, caveat, or question.
Hirai et al. (1996) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: