Hand lay-up was used to create banana and nylon Fibre-reinforced vinyl ester (VE) composites with random orientation of the short fibre ratio (banana:nylon = 1:1). To make it environmentally conscious, natural fibre (banana) was added in synthetic fibre (nylon). After fabrication, different mechanical testing was conducted. Tensile strength improves by 47% at 10 wt. % fibre loading and 13% at 20 wt.% fibre loading. Flexural strength improved by up to 213% at 15 wt. % fibre loading. At 20 wt. % fibre loading, the mean hardness number reaches its maximum. The mean impact energy is highest at 15 wt. % fibre loading. Furthermore, the highest water absorption is 2.3% with a fibre loading of 20 wt.%. After 15 wt.% fibre loading, which is suggested for optimal performance, the manufactured composites exhibit a declining trend in tensile, flexural, and impact capabilities. As a result, scanning electron micrographs were collected at 20 wt.% fibre loading to investigate the type of fibre-matrix bonding, voids, fibre agglomeration, and fibre pullouts phenomena. Fourier Transform Infrared spectroscopy was also explored to show a decline in hemicelluloses content. As-fabricated composites have several technological uses, including leisure and sports products, maritime sectors, and airplanes.
No takes yet. Share an insight, caveat, or question.
Haque et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: