Answers are grounded in this paper and cite their sources.
Ferroelectric lead-zirconate-titanate (PZT) thin films were deposited by excimer laser ablation on (100) MgO substrates with and without an electrode. The film composition was approximately the same as that of the target over a laser fluence range of 2.6 and 10 J/cm2·shot. Increase in the laser fluence enhances the film deposition rate and the crystallite size. In representative experiments, the remanent polarization and coercive field of the film prepared at a laser fluence of 9.2 J/cm2·shot were 28 µC/cm2 and 72 kV/cm, respectively.
No takes yet. Share an insight, caveat, or question.
Kidoh et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: