The flow and fracture mechanisms of well characterized hot‐pressed polycrystalline BeO were studied. Modulus of rupture tests were made from‐196O to 1800°C on specimens of constant density and varying grain size. The fracture surfaces were studied with fractography and X‐ray rocking curves. Compression tests were performed both below and above the phase transformation temperature for BeO (2050°C). A model was developed for fracture below 1000°C, involving propagation of existing surface cracks through dissimilar barriers to form a crack front of irregular shape which generates dislocations near the tip. Above 1000°C a model of grain boundary sliding to open cracks at grain boundary junctions was indicated. Permanent deformation under compression was attributed to grain separation and void formation.