Demonstrates atomic layer deposition of low-resistivity iridium thin films using a novel precursor with molecular oxygen, indicating optimal deposition temperatures between 275 and 300 °C.
Iridium thin films were grown by atomic layer deposition (ALD) between 225 and 350 °C using (MeCp)Ir(CHD) (MeCp = methylcyclopentadienyl, CHD = cyclohexadiene) and molecular oxygen as precursors. (MeCp)Ir(CHD) precursor was synthesized and characterized in-house. Also the crystal structure of (MeCp)Ir(CHD) is reported. All the ALD grown Ir films passed a common tape test indicating a good adhesion on Al2O3 nucleation layer. Quite untypically, surface roughness was the highest on films deposited at 225–250 °C and decreased strongly by increasing deposition temperature. Partial decomposition of the (MeCp)Ir(CHD) precursor resulted in defects on the film surface at 350 °C. Ir thin films with good quality were obtained at the deposition temperatures of 275 and 300 °C. A 50 nm thick film grown at 275 °C had a roughness of 1.2 nm, contained about 3 at% oxygen, 0.6 at% carbon and 1.6 at% hydrogen impurities, while the resistivity was as low as 9 µΩ cm.
No takes yet. Share an insight, caveat, or question.
Hämäläinen et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: