This is the authors' abstract. We don't add key points for this paper.
We successfully demonstrated a transition from a metallic InOx film into a nondegenerate semiconductor InOx:H film. A hydrogen-doped amorphous InOx:H (a-InOx:H) film, which was deposited by sputtering in Ar, O2, and H2 gases, could be converted into a polycrystalline InOx:H (poly-InOx:H) film by low-temperature (250 °C) solid-phase crystallization (SPC). Hall mobility increased from 49.9 cm2V−1s−1 for an a-InOx:H film to 77.2 cm2V−1s−1 for a poly-InOx:H film. Furthermore, the carrier density of a poly-InOx:H film could be reduced by SPC in air to as low as 2.4 × 1017 cm−3, which was below the metal–insulator transition (MIT) threshold. The thin film transistor (TFT) with a metallic poly-InOx channel did not show any switching properties. In contrast, that with a 50 nm thick nondegenerate poly-InOx:H channel could be fully depleted by a gate electric field. For the InOx:H TFTs with a channel carrier density close to the MIT point, maximum and average field effect mobility (μFE) values of 125.7 and 84.7 cm2V−1s−1 were obtained, respectively. We believe that a nondegenerate poly-InOx:H film has great potential for boosting the μFE of oxide TFTs.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Kataoka et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: