Answers are grounded in this paper and cite their sources.
The saturation magnetization values (Ms) of α-Fe∕Ba3Co1.8Fe23.6Cr0.6O41 nanocomposites prepared by mechanically alloying α-Fe with Ba3Co1.8Fe23.6Cr0.6O41 powders increased with increasing the concentration of α-Fe. α-Fe∕Ba3Co1.8Fe23.6Cr0.6O41 nanocomposites showed higher coercivity values than α-Fe and Ba3Co1.8Fe23.6Cr0.6O41 because of the effects of shape anisotropy and exchange bias. The resin compacts with 33.5 vol % α-Fe∕Ba3Co1.8Fe23.6Cr0.6O41 (38, 70, 85 vol % α-Fe) powders provided good electromagnetic wave absorption performances in ranges of 7.5–16.0, 5.4–10.5, and 4.3–8.3 GHz over the absorber thicknesses of 1.3–2.5, 1.6–3.0, and 1.7–3.2 mm, respectively.