The limiting long time static load carrying capability of an epoxy joint was found to depend on its ability to resist crack extension in the presence of water. This resistance to crack extension in an aggressive environment can be quantitatively described as the threshold of crack-extension-force below which stress corrosion cracking cannot occur, i.e. 𝒢iscc·- It was found for DER 332 hardened with TEPA that 𝒢iscc was approximately ⅓ to ½ 𝒢ic, the crack-extension-force in short times in the absence of water. The same resin hardened with HHPA had a value of 𝒢iscc that could be as low as 1/10 𝒢ic for the same system. For a particular resin system, 𝒢iscc was also found to be a function of relative humidity
No takes yet. Share an insight, caveat, or question.
Ripling et al. (1971) studied this question.