One of the techniques of severe plastic deformation, which has been used to improve the strength of the biocompatible zirconium alloy Zr–2.5% Nb (E125), is rotary forging. Swaging of an initially recrystallized alloy rod from a diameter of 12 mm to a diameter of 6.5 mm resulted in the formation of a grain–subgrain oriented microstructure characterized by a high density of dislocations and a predominance of low-angle misorientations of structural elements. These structural changes led to an increase in the yield strength and in the ultimate tensile strength of the alloy by a factor of 2.1 and 1.6, respectively. The alloy has a good plasticity margin after rotary swaging; the relative elongation is 14%. The complex of mechanical properties achieved for the Zr–2.5% Nb alloy meets the requirements for dental implant materials.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Рогачев et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: