This is the authors' abstract. We don't add key points for this paper.
Lead‐free BNT ‐based piezoceramics, (1− x ) Bi 0.5 Na 0.5 TiO 3 – x Bi ( Mg 0.5 Ti 0.5 ) O 3 [(1− x ) BNT – x BMT ] (0.00 ≤ x ≤ 0.06) binary system, were synthesized using a conventional ceramic fabrication method. Effect of Bi ( Mg 0.5 Ti 0.5 )O 3 ( BMT ) substitution on room temperature (RT) crystal structure, and temperature dependence of electric properties were investigated. The XRD indicates that a pure perovskite phase is formed. The introduction of BMT decreases E C of BNT from 7.3 to 4.0 kV/mm, and increases d 33 from 58 pC/N to 110 pC/N for the x = 0.05. The system shows a typical ferroelectric ( FE ) polarization loop P ( E ) and butterfly bipolar strain‐electric S ( E ) curve at RT. For the composition of 0.95 BNT –0.05 BMT antiferroelectric ( AFE ) phase appears near 80°C, characterized by a constricted P ( E ) loop and altered bipolar S ( E ) butterfly, and gradually prevails with increasing temperature. Temperature dependence of dielectric constant shows that T C increases from 310°C for pure BNT to 352°C for the x = 0.05. The results indicate that the piezoelectric properties of BNT have been improved by means of Bi ( Mg 0.5 Ti 0.5 ) O 3 substitution.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: