Answers are grounded in this paper and cite their sources.
Organosoluble montmorillonite/polyimide hybrids were prepared using a monomer solution intercalation polymerization method. Montmorillonite was organo-treated with p-aminobenzoic acid and the organosoluble polyimide was based on pyromellitic dianhydride and 4,4′-diamino-3,3′-dimethyldiphenylmethane. The particle size of montmorillonite in the hybrid containing 1 wt % of montmorillonite is about 400 nm. The strength and the toughness of montmorillonite/polyimide hybrids are improved simultaneously when the montmorillonite content is below 5 wt %. The thermal stabilities of montmorillonite/polyimide hybrids are obviously improved and their thermal expansion coefficients are reduced. When the montmorillonite content is below 5 wt %, the montmorillonite/polyimide hybrids are soluble in strong aprotonic polar organic solvents.
No takes yet. Share an insight, caveat, or question.
Zhu et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: