A recent review suggests that the commonly cited value of 1.45×1010 cm−3 for the silicon intrinsic carrier concentration at 300 K is inconsistent with the best experimental and theoretical results. An alternative value of 1.08×1010 cm−3 was suggested. A new experimental measurement of 1.01×1010 cm−3 is reported with an estimated one standard deviation uncertainty of only 3%. This appears to be the most accurate experimental determination of this parameter at any temperature.
No takes yet. Share an insight, caveat, or question.
Sproul et al. (1990) studied this question.