This is the authors' abstract. We don't add key points for this paper.
The β–type Ti–15Mo and Ti–15Mo–5Mn alloys were in situ synthesized on commercially pure Ti substrates via preplaced laser cladding of elemental powder blends. A systematic parameter screening revealed that Mn addition enables defect–free processing at significantly lower surface energy densities (1786–2143 J/cm²) compared to binary Ti–Mo alloys (6429–7500 J/cm²). Microstructural analysis showed that Mn promotes pronounced grain refinement (average grain size 40–58 µm vs. 116–129 µm for Mn–free alloys), attributed to solute redistribution and constitutional undercooling. EBSD confirmed β–phase predominance, with minor α/α′ fractions ranging from 0.64% to 5.44%, further stabilized by Mn addition. All alloys exhibited hardness substantially above the reference Ti–64 ELI alloy (325 HV), with values of 385–485 HV. Elastic modulus ranged from 104 to 118 GPa; the Ti–15Mo–5Mn alloy processed at 1786 J/cm² exhibited the lowest value (104 ± 8 GPa), combined with high hardness (450 HV) and a competitive H/E ratio (42.4 × 10⁻³), representing the most balanced property profile of all conditions evaluated. These results demonstrate that laser in situ alloying is a viable approach for producing low–modulus β–Ti alloys directly from elemental powders, with the Ti–15Mo–5Mn composition processed at optimized parameters emerging as a promising candidate for functionally graded orthopedic implants.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Lourenço et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: