Answers are grounded in this paper and cite their sources.
A 5 cm bore dia., 1-m-long dipole model magnet was constructed by winding un-reacted cable, followed by reaction and epoxy-impregnation. Experience and test results are described on the 1.7 mm dia. internal-tin wire, the eleven-strand flattened cable, fiberglass insulation, and construction of the magnet. Each half of the magnet has two double-pancake-type windings that were reacted in a single operation. The two double-pancakes were then separately vacuum impregnated after soldering the flexible Nb-Ti leads to the Nb3Sn conductors. No iron flux return yoke was used. In initial tests a central field of 8.0 T was reached at 4.4 K. However, evidence from training behavior, and 1.8 K tests indicate that premature quenching, rather than critical current of the cable, limited the field intensity. The magnet was reassembled and more rigidly clamped; additional test results are reported.
No takes yet. Share an insight, caveat, or question.
Taylor et al. (1985) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: