For Si single crystals irradiated with 150 MeV Ni+9 and Cl+9 ions, it was found by X-ray diffraction topographic observation that (1) two kinds of characteristic and systematic fringes can be seen in the irradiated area, (2) the surface of the specimen irradiated with Cl+9 was most damaged just behind the Al-mask of 34 µm thickness, rather than the directly irradiated area, and (3) the specimen is deformed after the irradiation and lattice strains are concentrated at the irradiation boundaries. The deformation and the strains were observed on the reverse surface of the irradiated crystal.
No takes yet. Share an insight, caveat, or question.
Hiroshi Tomimitsu (1983) studied this question.