Answers are grounded in this paper and cite their sources.
This study describes the synthesis of a hydroxyl silane coupling agent (HO‐silane) through a click reaction between SH in 3‐(trimethoxysilyl)propane‐1‐thiol (KH‐590) and CC in 2‐hydroxyethyl methacrylate (HEMA). This coupling agent was subsequently employed in the synthesis of silane‐modified polyurethane (SPU) resin which could be moisture‐cured at room temperature. The influence of r values (the molar ratio of NCO and OH) on the characteristics of SPU resins was investigated. These results reveal that an increase in the r value leads to a reduction in viscosity from 4.9 × 105 to 1.9 × 105 mPa·s, a rise in tensile strength from 0.88 to 0.98 Mpa followed by a decline to 0.69 MPa, and a reduction in extension at fracture from 236% to 94%. A SPU resin with a viscosity of approximately 3.6 × 105 mPa·s, tensile strength of 0.98 MPa, and elongation at break of 218% can be produced when the r value is 1.8. In addition, a silane‐modified polyurethane (MS) sealant with a tensile strength of 1.6 MPa in addition to elongation at break at 336% could be produced using the aforementioned SPU resin.
No takes yet. Share an insight, caveat, or question.
Guo et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: