Two approaches for the preparation of highly ionconductive polymeric solid electrolytes have been followed: one was to add crown ether to cross‐linked poly(ethylene oxide) grafted methacrylate polymer swollen by lithium salt/propylene carbonate solution; and the other was to select crosslinked poly(dimethylsiloxane) with a low glass transition temperature for the matrix material. The conductivity of the former electrolyte was 3.2 × 10−3 S/cm even in the absence of crown ether at 20°C and increased to 4.0 × 10−3 S/cm by the addition of 15‐Crown‐5. The addition of crown ether in the electrolyte also affected the plating and stripping processes of Lion Ni substrate. The latter electrolyte was prepared as a single ion type polymeric solid electrolyte. The conductivity of the electrolyte was ca 10−5 S/cm at room temperature. The polarization curves of Li in the electrolyte were symmetric for O V vs. Li/Li+, therefore the plating and stripping of Li electrode in the electrolyte were reversible. The behavior of the latter electrolyte is preferable for rechargeable lithium battery use.
No takes yet. Share an insight, caveat, or question.
Matsuda et al. (1993) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: