Sputter-deposited LaNiO3 (LNO) was used as a conductive buffer layer for the deposition of 80-nm-thick Ba0.4Sr0.6TiO3 (BST) thin films on Pt/Ti/SiO2/Si substrates by rf magnetron sputtering. Smooth and highly (100)-oriented perovskite films of BST were grown on the (100)-textured LNO by deposition at temperatures ≧200 °C. However, a relatively rough and weakly crystallized BST film was obtained by deposition directly on Pt/Ti/SiO2/Si substrates at 500 °C. Satisfactory dielectric constants of 160 to 320 were achieved for films deposited on LNO at temperatures from 350 to 550 °C, while a low dielectric constant of 120 was obtained for the film deposited on Pt at 500 °C. All the films in a Pt/BST/LNO or Pt/BST/Pt capacitor configuration basically showed a similar ohmic conduction characteristic of low conductivity in low bias regime up to a transition voltage around 1–3 V, and beyond that a nonohmic conduction with current rapidly increasing against the applied bias occurred. However, the films deposited on LNO would have a more moderate nonohmic conduction than that of the film deposited on Pt.
No takes yet. Share an insight, caveat, or question.
Wu et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: