This is the authors' abstract. We don't add key points for this paper.
Single crystals with the nominal composition of (Pr 0.01 ,Lu 0.99 ) 3 (Ga x ,Al 1- x ) 5 O 12 (Pr:LuGAG) were grown by the micro-pulling-down (µ-PD) method with RF heating and their luminescence properties were characterized. Transparent and crack free crystals that were slightly yellowish green were obtained. Lattice constants and densities systematically increased with increasing of Ga concentration. The luminescence properties of Pr:LuGAG were characterized by photoluminescence spectra and decays, radioluminescence spectra and light yield measurements. 5d–4f luminescence was observed for the x ≤0.6 samples. It was found that the 5d–4f emission of Pr 3+ is quenched only slightly up to x ≤0.4 whereas density systematically increased in the range of 0≤ x ≤1.0.
No takes yet. Share an insight, caveat, or question.
Ogino et al. (2007) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: