Answers are grounded in this paper and cite their sources.
TiN films were deposited by remote plasma-enhanced atomic layer deposition (PEALD) and a metalorganic chemical vapor deposition (MOCVD) method with post-plasma-treatment using the same precursor, tetrakis (dimethylamino)titanium (TDMAT), as a Ti source. In remote PEALD, the plasmas of hydrogen, nitrogen, and ammonia were used, while in MOCVD, the ammonia gas was used as a reactant and followed by the post-plasma-treatment with hydrogen or nitrogen. The TiN films deposited by remote PEALD showed a relatively constant compositional variation with carbon impurity contents less than 5 atom %. The TiN film exhibited amorphous phase at annealing temperatures up to 500°C and transferred to a crystalline phase after annealing above 550°C. The measured growth rate of TiN films was about 2θ per cycle. The TiN films also showed excellent step coverage above 95% with a very high aspect ratio structure. The TiN film deposited by remote PEALD exhibited almost uniform compositional variation in depth with less than 3 atom % carbon impurity at the top and side of contact hole. However, the TiN films deposited by MOCVD with post-plasma-treatment showed nonuniform compositional variations depending on the positions with about 5 and 10 atom % carbon impurity at the top and side on contact hole, respectively.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2004) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: