The growth mechanism of the passivation layer in the cryogenic process used for silicon deep etching is explored experimentally in an inductively coupled plasma reactor. In particular, the role of SiF 4 etching by-products on the SiO x F y layer deposition is investigated. The deposition of a SiO x F y layer using SiF 4 and O 2 gases is studied by in situ ellipsometric spectroscopy in different experimental configurations to devise the deposition mechanism: SiF 4 /O 2 plasma mixture, alternation of SiF 4 plasma and O 2 plasma steps and alternation of SiF 4 flow without plasma and O 2 plasma steps. The refractive index and the thickness of the deposited layer are measured for different substrate temperatures, from −125 °C to 20 °C. Although some of the passivation layer is removed during the wafer warm up, a residual amount remains at the surface. The deposited SiO x F y layer forms more efficiently at low temperature with an optimal temperature of −100 °C in our experimental conditions. The passivation layer was etched by a SF 6 plasma without bias versus the deposition temperature, to evaluate its resistance to plasma etching steps. The passivation layer was analyzed by ex situ EDX and XPS. We investigated the role of SiF 4 low temperature physisorption in the formation of the passivation layer on the sidewalls of the features that are being etched, which are not submitted to ion bombardment. It is shown that physisorption of SiF x species play an important role because their residence time at the surface is longer, thus increasing the probability of reaction with oxygen.
No takes yet. Share an insight, caveat, or question.
Antoun et al. (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: