Fully dense isotropic Sm-Fe-N magnets were successfully fabricated using the shock-wave consolidation method. Deterioration of hard magnetic properties of the Sm-Fe-N by the impact load during the consolidation process was not observed, and consequently, the fully dense magnet showed high (BH)max of 116–144 kJ/m3 (14.5–18.0 MGOe) which is the highest level among all the isotropic magnets. Its temperature coefficient ofBᵣwas 0.066%/°C and that of coercivity was 0.36%/°C. The irreversible flux loss of the sample with$L/D$of 0.78 after exposed at 150 °C was a small value of 5%–10%. The fully dense Sm-Fe-N magnet without coating showed a good corrosion resistance, and it had enough mechanical strength. The volume resistivity of the consolidated Sm-Fe-N magnet with a packing ratio of 97.4% was2.8 ~μ Ω · m. From these results, the practicality of the fully dense Sm-Fe-N magnet made by shock-wave consolidation has been confirmed.
No takes yet. Share an insight, caveat, or question.
Takagi et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: