Answers are grounded in this paper and cite their sources.
A bicrystal of Zn with an originally flat 89° 〈101̄0〉 symmetric tilt boundary was annealed in a magnetic field of 25 T. The boundary migrated under the action of a magnetic driving force in the direction of the grain with higher diamagnetic susceptibility. In addition, the boundary changed its crystallographic orientation, decreasing length and becoming almost perpendicular to the free surfaces. The results were interpreted in terms of magnetically forced grain boundary motion due to the anisotropy of the magnetic susceptibility in Zn. The absolute boundary mobility was measured to be about 5.1×10−9 m4/J s.
No takes yet. Share an insight, caveat, or question.
Sheikh‐Ali et al. (2003) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: