The variation amount of TiO 2 at 1, 3 and 5 mol% was added into 0.93(Bi0.5Na0.5)TiO3-0.07Ba(Ti0.95Zr0.05)O3, (BNT-7BZT) powder. The affect of excess TiO2 on ferroelectric properties of BNT-7BZT ceramics were studied. It was found that piezoelectric and dielectric constants as well as dissipation factor largely drop with an increase of TiO2 contents. However, TiO2 excess can stabilize the curie temperature and give a first phase transition temperature constantly at 125°C with TiO2 more than 1 mol%.