The variety of wide‐angle x‐ray scattering (WAXS) patterns exhibited by nylon‐6 fibers with different fabrication histories is rationalized using a model comprising three limiting structures, viz., an α, a γ, and a pleated α structure. The γ and pleated α structures both have a single broad reflection in the range 2θ = 19° −25°, but differ in their annealing behavior. At 205° (in vacuo), the pleated α structure converts to the normal α structure by removal of the pleats, without breaking any hydrogen bonds. The γ structure, however, remains unchanged under this annealing condition since it is necessary to break all the hydrogen bonding in the structure to convert it to the α form. Different fabrication routes produce fibers which resemble the three ideal structures to varying extents. Fibers extruded at low speeds (and hence low spinline tension) resemble a mixed conventional α/pleated α structure with only a small γ component. Increasing the take‐up speed (and hence the spinline tension) of the as‐spun fiber, or in‐line drawing of the low orientation fiber (without prior storage), increases the γ content. If drawing of the low orientation fiber takes place after several hours storage (off‐line drawing), a largely α structure is produced. The intensity of the 020 reflection in the γ structure is shown to be very dependent on the degree of crystalline orientation in the sample.
No takes yet. Share an insight, caveat, or question.
Stepaniak et al. (1979) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: