Spark plasma sintering technique had been applied to prepare bulk isotropic and anisotropic nanostructured Nd–Fe–B permanent magnets via hot pressing and subsequent hot deformation process. Influences of processing conditions and deformation height reduction on the structure and magnetic properties of the magnets were investigated. For the hot deformed magnet with 80% height reduction, XRD patterns of the anisotropic magnets show dominant (00l) diffraction peaks indicating evident c-axis crystallographic alignment in the magnet. Under the optimal processing conditions, the anisotropic magnet with 80% height reduction exhibits excellent magnetic properties as remanence (Br) of 1.492 T, coercive force (Hci) of 1004 kA/m, and the maximum energy product [(BH)max] of 400 kJ/m3, which are among the highest reported magnetic properties of nanostructured Nd–Fe–B permanent magnets.
No takes yet. Share an insight, caveat, or question.
Liu et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: