Vanadium pentoxide was deposited by atomic layer deposition (ALD) from vanadyl-tri-isopropoxide (VTIP). Water or oxygen was used as a reactive gas in thermal and plasma-enhanced (PE) processes. For PE ALD, there was a wide ALD temperature window from 50 to . Above , VTIP decomposed thermally, resulting in the chemical vapor deposition (CVD) of vanadium pentoxide. The PE ALD reactions saturated much faster than during thermal ALD, leading to a growth rate of approximately 0.7 Å/cycle during PE ALD using or . Optical emission spectroscopy showed combustion-like reactions during the plasma step. X-ray diffraction was performed to determine the crystallinity of the films after deposition and after postannealing under He or atmosphere. Films grown with CVD at and PE ALD at were (001)-oriented as deposited, while thermal and PE ALD films grown at were amorphous as deposited. The crystallinity of the PE ALD could be correlated to its high purity, while the other films had significant carbon contamination, as shown by X-ray photoelectron spectroscopy. Annealing under He led to oxygen-deficient films, while all samples eventually crystallized into under .
No takes yet. Share an insight, caveat, or question.
Musschoot et al. (2009) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: