Answers are grounded in this paper and cite their sources.
The effects of alpha-Ti depositions, caused with the heat treatments at 300-500degC, were studied for various V-Ti alloys through measurements of Tc, Ic, and X-ray diffraction patterns. Jcincreased with the alpha-Ti depositions for the V-Ti alloys with various Ti contents. The alpha-Ti depositions are very effective pinning centers in V-Ti alloys, being similar to those in Nb-Ti alloys. The maximum Tc of 8.2 K was obtained for the V-40at%Ti alloy annealed at 500degC for 2 hr, while the maximum Birr(4.2 K) of 8.5 T was obtained for the V-(50-60) at%Ti alloys. Jc(4.2 K, and 6.5 T) of about 170 A/mm2was obtained for the V-45at%Ti alloy annealed at 500deg C for 4 hr. We also fabricated the V-Ti alloy multifilament;!!} wires in order to stabilize the alloy superconductors. The final cold-drawing after heat treatment at 400-450degC is effective on the improvements of Tc, Birr, and Jcof the multifilamentary V-(40-45)at%Ti alloy wires. Jc(4.2 K, 6.5 T) of 200 A /mm2was obtained for the multifilamentary wire.
No takes yet. Share an insight, caveat, or question.
Tai et al. (2007) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: