This paper investigates the creep properties of lead-free (Sn3.8Ag0.7Cu) and lead-containing (Sn37Pb) solder alloys. To simulate the working environment of solder joints in a Microelectronic Packaging Module (EPM), creep failure was estimated using isothermal and combined thermal-mechanical fatigue tests on Ball Grid Array (BGA) specimens over the temperature range 25−75∘C. A steady-state power law creep relationship was employed to determine creep parameters, including stress exponent and activation energy. The results showed that creep exponent (n) increases with temperature in lead-free Sn3.8Ag0.7Cu and decreases in lead-containing Sn37Pb solders. The activation energy and average creep exponent of lead-free solder were, respectively, ∼7% and ∼105% greater than those of lead-containing solder, indicating that Sn3.8Ag0.7Cu alloy has better creep resistance compared to the Sn37Pb solder. The potential sustainability advantages associated with the improved creep resistance of Sn3.8Ag0.7Cu solder are discussed.
No takes yet. Share an insight, caveat, or question.
Ghaleeh et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: