This research aimed to study the bending behavior of self-compacting concrete (SCC) beams reinforced with steel fiber and B500 ribbed reinforcing bar. The studied variables were four: cracking patterns and failure mode, effect of main reinforcement area, effect of rebar grades, and effect of fiber content. Six rectangular beams of cross section of size 100×200 mm and a length of 2000 mm were casted and tested under four-point bending. One beam was used as a control beam without steel fibers, while the other five beams were casted using steel fibers. The steel fiber content was varied from zero to 25 and 50 kg/m3. Three types of rebar main reinforcement were used B500DWR, B500CWR, and B500C-R. According to the experimental results, the tensile strain at failure load ranged from 64,4.7 and 99.2% of that of control beam B1 and the compressive strain at failure load was 76.2 % and 57.1 % of that of beam B1, the control beam. The failure load for beams were 101.5.3 and 106.7 % of that of the control beam B1. Changing the main reinforcement for beams lead to the maximum deflection for beams ranged from 101.5, 109.9, and 81.3% of that of the control beam.
No takes yet. Share an insight, caveat, or question.
sadek et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: