Thermally-activated, liquid-based crack healing was investigated using a magnetron sputtered Al / Sn / Al thin film architecture with Sn acting as the healing agent. A brittle Al2O3 layer was sputtered prior to the deposition of the Al and Sn layers enabling the formation of cracks with varying widths in the Al layers (2–4 μm) using a 3-point bending technique. Thermal activation was achieved through annealing at 250°C for 10 min and 400°C for 10 and 30 min. Scanning transmission electron microscopy imaging revealed that Sn mobility was activated only after annealing at 400°C for 30 min. resulting in efficient healing of ~2 μm wide cracks, while >3 μm wide cracks showed a reduced healing efficiency in comparison. The here observed variations in healing efficiency are governed by the temperature-dependent wetting behavior of Al by Sn as well as by crack-width-dependent capillary forces and the healing time. This study provides insights into the fundamental mechanisms governing liquid-based self-healing in metals, contributing towards future knowledge-driven design of self-healing bulk metals and metallic thin films.
No takes yet. Share an insight, caveat, or question.
Mráz et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: