samples having a modulus of 43 kPa and reaching an extension ratio of 8.5 and a fracture stress of 175 kPa. This enhanced elasticity is thought to be brought about by a combination of coiled but only weakly-entangled PAA chains with phase-separated regions of salt acting as a plasticizer and modulating intermolecular interactions among AA units.