Photolithographically-defined patterned arrays of Co-rich Co-Pt permanent magnets with thicknesses up to 10 mu m were fabricated by aqueous electrodeposition. These micromagnets exhibited strong perpendicular magnetic performance while being deposited at low temperatures (65degC) and without the need for post-deposition annealing. Co-Pt magnet arrays grown 10-mu m thick on textured Cu (111) seed layers on Si (110) substrates exhibited coercivities of 330 kA/m (4.1 kOe) and energy products 69 kJ/m3. Additionally, magnets deposited 8-mu m thick on untextured Cu seed layers on standard Si (100) substrates exhibited coercivities up to 260 kA/m (3.3 kOe) and energy products up to 27 kJ/m3. The high magnetic performance and process integrability of these permanent magnet arrays make them well suited for the development of magnetic microelectromechanical systems (MEMS).
No takes yet. Share an insight, caveat, or question.
Wang et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: