Magnetic properties of melt-spun Co80Zr20−xBx microcrystalline alloys (0≤x≤8) depend crucially on the quench rate.The optimized values of Hc =2.68 kOe and (BH)max =2.10 MG Oe were obtained for Co80Zr16B4 melt-spun with the substrate surface velocity of 48 m/s. A new crystalline phase of Co5Zr was observed.
No takes yet. Share an insight, caveat, or question.
Stroink et al. (1990) studied this question.