Alumina ceramics possess excellent thermal, chemical, and mechanical properties but usually require sintering above 1600 °C, leading to high energy use and grain growth. Commercial alumina (95–96% purity) with conventional SiO 2 –MgO–CaO additives is also typically sintered at ≥1600 °C. In this study, a synergistic combination of a ternary oxide sintering aid (5 wt.% CuO–TiO 2 –Nb 2 O 5 ) and spark plasma sintering (SPS) was used to drastically lower the densification temperature of alumina. Fully dense alumina (≈100%) was achieved at 750 °C under 60 MPa and at 850 °C under 10 MPa, compared with pressureless sintering, which reached only 97% density at 1050 °C. SPS created a reductive environment that stabilised Cu + species and promoted liquid-phase-assisted densification while suppressing abnormal grain growth. In contrast, pressureless sintering led to CuO migration and niobium-rich secondary phases. SPS-processed samples showed finer, more uniform grains and comparable or higher hardness. Overall, combining ternary oxide additives with SPS enables energy-efficient, ultra-low-temperature densification of alumina with controlled microstructure.
No takes yet. Share an insight, caveat, or question.
Stosz et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: